EFFECTS OF POST-WELD HEAT TREATMENT ON THE MICROSTRUCTURAL EVOLUTION AND MECHANICAL PROPERTIES OF DISSIMILAR FRICTION STIR WELDED AA6061+SICP/AA6061-O JOINT

Authors

  • NAHIT OZTOPRAK THE GRADUATE SCHOOL OF NATURAL AND APPLIED SCIENCES, DOKUZ EYLUL UNIVERSITY, IZMIR, TURKEY HTTP://ORCID.ORG/0000-0003-1132-8768
  • CINAR EMINE YENI DEPARTMENT OF MECHANICAL ENGINEERING, DOKUZ EYLUL UNIVERSITY, IZMIR, TURKEY
  • BINNUR GOREN KIRAL DEPARTMENT OF MECHANICAL ENGINEERING, DOKUZ EYLUL UNIVERSITY, IZMIR, TURKEY

Abstract

A RESEARCH ON THE MICROSTRUCTURE AND MECHANICAL PROPERTIES OF THE DISSIMILAR JOINT WAS CARRIED OUT SO AS TO UNDERSTAND THE EFFECTS OF POST-WELD HEAT TREATMENT (PWHT) ON MICROSTRUCTURAL EVOLUTION, MICROHARDNESS, TENSILE AND FLEXURAL PROPERTIES OF THE DISSIMILAR FRICTION STIR WELDED (FSWED) JOINT. THE RESULTS SHOWED THAT THERE IS A SUFFICIENT AND RATHER COMPLICATED MATERIAL MIXING IN THE NUGGET ZONE (NZ). AFTER PWHT, THE GRAINS IN THE JOINT AREA EXCEPT FOR THE NZ DEMONSTRATED A GRAIN REFINEMENT WITH MORE HOMOGENEOUS AND EQUIAXED GRAINS. FINE AND CLUSTERED SIC PARTICLES IN THE NZ ARE CON-FIRMED BY SCANNING ELECTRON MICROSCOPE (SEM). IN ADDITION, THE MICROHARDNESS VALUES OF NUGGET ZONES BOTH IN AS-WELDED AND PWHT CONDITION EXHIBITED A HIGHER VICKERS COMPARED TO THAT OF AA6061-O. FURTHERMORE, A MAXIMUM TENSILE STRENGTH OF 183.30 MPA THAT DEMONSTRATES A 52.22% INCREASE IN TENSILE STRENGTH IS ALSO OBSERVED IN THE TRANSVERSE TENSILE TESTS SUBSEQUENT TO PWHT. CONSIDERING THE THREE-POINT BENDING TEST RESULTS, IT IS EXPLICIT THAT AN INCREASE OF 121.96% IN THE BENDING EXTENSION IS OBTAINED AS THERE IS NO SIGNIFI-CANT INCREASE IN MAXIMUM BENDING FORCE AFTER THE PWHT.

Downloads

Published

2018-02-02

Issue

Section

Articles